Atomic Layer Deposition (ALD) Maryam Ebrahimi University of Waterloo January 17 th, 2006 Chem 750/7530 1
Outline • • • ALD Theory and Process Precursor Requirements Deposition Advantages Comparison to CVD Process Applications 2
What is ALD? • ALD (Atomic Layer Deposition) • Deposition method by which precursor gases or vapors are alternately pulsed on to the substrate surface. • Precursor gases introduced on to the substrate surface will chemisorb or surface reaction takes place at the surface • Surface reactions on ALD are complementarity and self-limiting 3
ALD Example Cycle for Al 2 O 3 Deposition Tri-methyl aluminum Al(CH 3)3(g) Methyl group (CH 3) Al C H Hydroxyl (OH) from surface adsorbed H 2 O H O Substrate surface (e. g. Si) • • • In air H 2 O vapor is adsorbed on most surfaces, forming a hydroxyl group. With silicon this forms : Si-O-H After placing the substrate in the reactor, Trimethyl Aluminum (TMA) is pulsed 4 into the reaction chamber
ALD Cycle for Al 2 O 3 Methane reaction product CH 4 H Reaction of TMA with OH H H C C H H Al O Substrate surface (e. g. Si) • Trimethyl Aluminum (TMA) reacts with the adsorbed hydroxyl groups, producing methane as the reaction products Al(CH 3)3 (g) + : Si-O-H (s) : Si-O-Al(CH 3)2 (s) + CH 4 5
• • ALD Cycle for Al 2 O 3 Trimethyl Aluminum (TMA) reacts with the adsorbed hydroxyl groups, until the surface is passivated. TMA does not react with itself, terminating the reaction to one layer. This causes the perfect uniformity of ALD. The excess TMA is pumped away with the methane reaction product. 6
ALD Cycle for Al 2 O 3 • After the TMA and methane reaction product is pumped away, water vapor (H 2 O) is pulsed into the reaction chamber. 7
ALD Cycle for Al 2 O 3 • H 2 O reacts with the dangling methyl groups on the new surface forming Aluminum-oxygen (Al-O) bridges and hydroxyl surface groups, waiting for a new TMA pulse. Again methane is the reaction product. 2 H 2 O (g) + : Si-O-Al(CH 3)2 (s) : Si-O-Al(OH)2 (s) + 2 CH 4 8
ALD Cycle for Al 2 O 3 • The reaction product methane is pumped away. Excess H 2 O vapor does not react with the hydroxyl surface group, again causing perfect passivation to one atomic layer. 9
ALD Cycle for Al 2 O 3 One TMA and one H 2 O vapor pulse form one cycle. Here three cycles are shown, with approximately 1 Angstrom per cycle. Each cycle including pulsing and pumping takes e. g. 3 sec. Two reaction steps in each cycle: Al (CH 3)3 (g) + : Al-O-H 2 H 2 O (g) + : O-Al(CH 3)2 (s) : Al-O-Al(CH 3)2 (s) : Al-O-Al(OH)2 + CH 4 (s) + 2 CH 4 10
ALD Precursor Requirements ü Must be volatile and thermally stable ü Preferably liquids and gases ü Should Chemisorb onto the surface or rapidly react with surface and react aggressively with each other -Short saturation time, good deposition rate, no gas phase reactions ü Should not self-decompose - Affect thickness, uniformity ü Should not etch, dissolute into film or substrate 11
Deposition Advantages Alternating reactant exposure creates unique properties of deposited coatings: Ø Thickness is determined simply by number of deposition cycles Ø Precursors are saturatively chemisorbed → stochiometric films with large area uniformity and 3 D conformality Ø Intrinsic deposition uniformity Ø Low temperature deposition possible Ø Gentle deposition process for sensitive substrate 12
Comparison of ALD and CVD • • • ALD Highly reactive precursors Precursors react separately on the substrate Precursors must not decompose at process temperature Uniformity ensured by the saturation mechanism Thickness control by counting the number of reaction cycles Surplus precursor dosing acceptable CVD • Less reactive precursors • Precursors react at the same time on the substrate • Precursors can decompose at process temperature • Uniformity requires uniform flux of reactant and temperature • Thickness control by precise process control and monitoring • Precursor dosing important 13
ALD Applications summary Piezoelectric layers (Zn. O, Al. N, Zn. S) High-k dielectrics (Al 2 O 3, Hf. O 2, Zr. O 2, Ta 2 O 5, La 2 O 3, ) for transistor gates and DRAM capacitors in Si, Ga. As, Heterostructures, compound semiconductors, Mesfets, III-V Semiconductor materials, organic transistors, graphene, graphite, nanotubes, nanowires, molecular electronics, Transparent Electrical Conductors (Zn. O: Al, ITO) UV blocking layers (Zn. O, Ti. O 2) OLED passivation (Al 2 O 3) Solid Lubricant layers (WS 2, ) Conductive gate electrodes (Ir, Pt, Ru, Ti. N, ) Photonic crystals (Zn. O, Zn. S: Mn, Ti. O 2, Ta 2 N 5, ) coatings inside porous alumina, inverted opals Metal interconnects and liners (Cu, WN, Ta. N, WNC, Ru, Ir) Metallic diffusion barrier layers for copper interconnects and semiconductor vias for transistor gate and memory cell applications, DRAM capacitors, Passivation layers Anti-reflection and optical filters (Al 2 O 3, Zn. S, Sn. O 2, Ta 2 O 5) Fabry-Perot, Rugate, Flip-Flop optical filters Catalytic materials (Pt, Ir, Co, Ti. O 2, V 2 O 5) Coatings inside filters, membranes, catalysts (thin economical Pt for automobile catalytic converters), fuel cells ion exchange coatings Nanostructures (all materials) Conformal deposition around and inside nanostructures and MEMS Biomedical coatings: (Ti. N, Zr. N, Cr. N, Ti. Al. N, Al. Ti. N) Biocompatible materials for in-vivo medical devices and instruments ALD metals (Ru, Pd, Ir, Pt, Rh, Co, Cu, Fe, Ni) Electroluminescent devices (Sr. S: Cu, Zn. S: Mn, Zn. S: Tb, Sr. S: Ce) Processing layers (Al 2 O 3, Zr. O 2, Etch barriers, ion diffusion barriers, fill layers for magnetic read heads Optical applications (Al. Ti. O, Sn. O 2, Zn. O) Photonics, Nanophotonics, Solar cells, integrated optics, optical coatings, lasers, variable dielectric constant nanolaminates Sensors (Sn. O 2, Ta 2 O 5, ) Gas sensors, p. H sensors, Wear and corrosion inhibiting layers (Al 2 O 3, Zr. O 2) 14
References • Cambridge Nano. Tech Inc. , Cambridge, MA 02139 USA www. cambridgenanotech. com/. . . / Atomic%20 Layer%20 Deposition%20 tutorial%20 Cambrid ge%20 Nano. Tech%20 Inc. pdf • www. mne. umd. edu/. . . /465_spring_2003/465_ spr 2003_final_project_results/ALD-finalpres-465 spr 2003. pdf • ICKNOWLEDGE LLC, Georgetown, MA 01833, www. icknowledge. com/misc_technology/ Atomic%20 Layer%20 Deposition%20 Briefing. pdf • B. S. Lim, A. Rahtu and R. G. Gordon, Nature Materials, 2 (2003) 749 -754 15